MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wieland Euro 50 PFM Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Palladium Alloy

Material Notes: Gold-palladium ceramic alloy

Applications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneering

Dental

Key Words: EN ISO 9693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.1 g/cc0.509 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 210210HV5/30; after porcelain firing
 240240HV5/30; hardened
Tensile Strength, Yield  489.9 MPa
@Strain 0.2 %
71050 psi
@Strain 0.2 %
after porcelain firing
 529.9 MPa
@Strain 0.2 %
76850 psi
@Strain 0.2 %
hardened
Elongation at Break 12 %12 %hardened
 14 %14 %after porcelain firing
Modulus of Elasticity 114 GPa16500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.7 µm/m-°C
@Temperature 25.0 - 500 °C
8.17 µin/in-°F
@Temperature 77.0 - 932 °F
Melting Point 1200 - 1280 °C2190 - 2330 °F
Solidus 1200 °C2190 °F
Liquidus 1280 °C2330 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 849 °C1560 °FPreheating Temp.
Casting Temperature 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 51.5 %51.5 %
Indium, In 0.90 %0.90 %
Palladium, Pd 26.6 %26.6 %
Ruthenium, Ru 0.10 %0.10 %
Silver, Ag 18.2 %18.2 %
Tin, Sn 2.7 %2.7 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
HGC-3-C Precious dental alloy
Wieland Auropal 1 Casting Alloy
Wieland BioPorta G PFM Alloy
Wieland Porta Maximum PFM Alloy

NWIELAN08 / 19810

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.