MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyphenylene Ether, 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 - 1.38 g/cc0.0448 - 0.0499 lb/in³Average value: 1.30 g/cc Grade Count:42
Filler Content 30.0 %30.0 %Average value: 30.0 % Grade Count:4
Water Absorption 0.0100 - 0.500 %0.0100 - 0.500 %Average value: 0.107 % Grade Count:17
Moisture Absorption at Equilibrium 0.0400 - 0.0600 %0.0400 - 0.0600 %Average value: 0.0550 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm0.00100 - 0.00600 in/inAverage value: 0.00245 cm/cm Grade Count:28
Linear Mold Shrinkage, Transverse 0.00200 - 0.00800 cm/cm0.00200 - 0.00800 in/inAverage value: 0.00400 cm/cm Grade Count:10
Melt Flow 1.00 - 30.0 g/10 min1.00 - 30.0 g/10 minAverage value: 11.5 g/10 min Grade Count:19
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 87.0 - 89.087.0 - 89.0Average value: 88.3 Grade Count:3
Ball Indentation Hardness 130 - 205 MPa18900 - 29700 psiAverage value: 166 MPa Grade Count:4
Tensile Strength, Ultimate 73.0 - 152 MPa10600 - 22000 psiAverage value: 106 MPa Grade Count:32
 40.0 - 80.0 MPa
@Temperature 60.0 - 120 °C
5800 - 11600 psi
@Temperature 140 - 248 °F
Average value: 60.0 MPa Grade Count:2
Tensile Strength, Yield 70.0 - 152 MPa10200 - 22000 psiAverage value: 116 MPa Grade Count:12
Elongation at Break 1.00 - 8.00 %1.00 - 8.00 %Average value: 3.40 % Grade Count:37
 1.50 - 2.80 %
@Temperature 60.0 - 120 °C
1.50 - 2.80 %
@Temperature 140 - 248 °F
Average value: 2.17 % Grade Count:2
Elongation at Yield 1.00 - 2.00 %
@Temperature 120 - 120 °C
1.00 - 2.00 %
@Temperature 248 - 248 °F
Average value: 1.50 % Grade Count:2
Modulus of Elasticity 4.10 - 10.5 GPa595 - 1520 ksiAverage value: 8.10 GPa Grade Count:22
 4.30 - 7.80 GPa
@Temperature 60.0 - 120 °C
624 - 1130 ksi
@Temperature 140 - 248 °F
Average value: 6.02 GPa Grade Count:2
Flexural Yield Strength 116 - 248 MPa16800 - 36000 psiAverage value: 163 MPa Grade Count:30
Flexural Modulus 2.82 - 10.5 GPa409 - 1520 ksiAverage value: 6.97 GPa Grade Count:35
Izod Impact, Notched 0.686 - 1.30 J/cm1.29 - 2.44 ft-lb/inAverage value: 1.00 J/cm Grade Count:26
 0.5339 - 1.1768 J/cm
@Temperature -40.0 - -30.0 °C
1.000 - 2.2046 ft-lb/in
@Temperature -40.0 - -22.0 °F
Average value: 0.819 J/cm Grade Count:3
Izod Impact, Unnotched 3.20 - 6.41 J/cm6.00 - 12.0 ft-lb/inAverage value: 4.34 J/cm Grade Count:4
Charpy Impact Unnotched 1.80 - 7.00 J/cm²8.57 - 33.3 ft-lb/in²Average value: 3.41 J/cm² Grade Count:8
 2.00 - 6.00 J/cm²
@Temperature -30.0 - -20.0 °C
9.52 - 28.6 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 3.50 J/cm² Grade Count:3
Charpy Impact, Notched 0.500 - 1.40 J/cm²2.38 - 6.66 ft-lb/in²Average value: 0.757 J/cm² Grade Count:16
 0.600 - 0.700 J/cm²
@Temperature -30.0 - -20.0 °C
2.86 - 3.33 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.633 J/cm² Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm1.00e+11 - 1.00e+17 ohm-cmAverage value: 2.79e+16 ohm-cm Grade Count:19
Surface Resistance 1.00e+13 - 6.00e+15 ohm1.00e+13 - 6.00e+15 ohmAverage value: 1.70e+15 ohm Grade Count:12
Dielectric Constant 2.90 - 3.502.90 - 3.50Average value: 3.07 Grade Count:6
Dielectric Strength 17.0 - 46.0 kV/mm432 - 1170 kV/inAverage value: 25.5 kV/mm Grade Count:10
Dissipation Factor 0.00100 - 0.009200.00100 - 0.00920Average value: 0.00336 Grade Count:5
Comparative Tracking Index 4.00 - 250 V4.00 - 250 VAverage value: 184 V Grade Count:11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 70.0 µm/m-°C11.1 - 38.9 µin/in-°FAverage value: 33.8 µm/m-°C Grade Count:13
CTE, linear, Transverse to Flow 50.0 - 61.0 µm/m-°C27.8 - 33.9 µin/in-°FAverage value: 57.4 µm/m-°C Grade Count:7
Thermal Conductivity 0.173 - 0.280 W/m-K1.20 - 1.94 BTU-in/hr-ft²-°FAverage value: 0.241 W/m-K Grade Count:5
Maximum Service Temperature, Air 85.0 - 160 °C185 - 320 °FAverage value: 131 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 120 - 255 °C248 - 491 °FAverage value: 169 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 115 - 241 °C239 - 466 °FAverage value: 152 °C Grade Count:37
Vicat Softening Point 132 - 220 °C270 - 428 °FAverage value: 151 °C Grade Count:14
Minimum Service Temperature, Air -40.0 - -20.0 °C-40.0 - -4.00 °FAverage value: -37.5 °C Grade Count:8
UL RTI, Electrical 65.0 °C149 °FAverage value: 65.0 °C Grade Count:3
UL RTI, Mechanical with Impact 65.0 °C149 °FAverage value: 65.0 °C Grade Count:3
UL RTI, Mechanical without Impact 65.0 °C149 °FAverage value: 65.0 °C Grade Count:3
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:28
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 - 282 °C450 - 540 °FAverage value: 264 °C Grade Count:5
Nozzle Temperature 270 - 325 °C518 - 617 °FAverage value: 295 °C Grade Count:4
Melt Temperature 249 - 320 °C480 - 608 °FAverage value: 289 °C Grade Count:14
Mold Temperature 50.0 - 121 °C122 - 250 °FAverage value: 89.8 °C Grade Count:19
Drying Temperature 80.0 - 120 °C176 - 248 °FAverage value: 94.4 °C Grade Count:14
Moisture Content 0.0200 - 0.100 %0.0200 - 0.100 %Average value: 0.0550 % Grade Count:4
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Overview of materials for Polyphenylene Ether, Heat Resistant
Overview of materials for Polyphenylene Ether, Impact Grade
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polyphenylene Ether, 10% Glass Filled

O4413 / 78325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.