MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gallium, Ga
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density  5.445 g/cc
@Temperature 1100 °C
0.1967 lb/in³
@Temperature 2010 °F
Liquid
 5.492 g/cc
@Temperature 1010 °C
0.1984 lb/in³
@Temperature 1850 °F
Liquid
 5.72 g/cc
@Temperature 600 °C
0.207 lb/in³
@Temperature 1110 °F
Liquid
 5.779 g/cc
@Temperature 500 °C
0.2088 lb/in³
@Temperature 932 °F
Liquid
 5.9037 g/cc
@Temperature 29.65 °C
0.21328 lb/in³
@Temperature 85.37 °F
Solid
 5.907 g/cc
@Temperature 20.0 °C
0.2134 lb/in³
@Temperature 68.0 °F
Solid
 5.972 g/cc
@Temperature 200 °C
0.2158 lb/in³
@Temperature 392 °F
Liquid
 6.093 g/cc
@Temperature 32.4 °C
0.2201 lb/in³
@Temperature 90.3 °F
Liquid
 6.0947 g/cc
@Temperature 29.8 °C
0.22018 lb/in³
@Temperature 85.6 °F
Liquid
Vapor Pressure  6.281e-9 bar
@Temperature 727 °C
0.000004711 torr
@Temperature 1340 °F
 0.000001279 bar
@Temperature 927 °C
0.0009593 torr
@Temperature 1700 °F
 0.00005636 bar
@Temperature 1127 °C
0.04227 torr
@Temperature 2061 °F
 0.0009572 bar
@Temperature 1327 °C
0.7180 torr
@Temperature 2421 °F
 0.00859 bar
@Temperature 1527 °C
6.44 torr
@Temperature 2781 °F
 0.04932 bar
@Temperature 1727 °C
36.99 torr
@Temperature 3141 °F
 0.205 bar
@Temperature 1927 °C
154 torr
@Temperature 3501 °F
 1.00 bar
@Temperature 2204 °C
750 torr
@Temperature 3999 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 69.72369.7231995
Atomic Number 3131
Thermal Neutron Cross Section 2.8 barns/atom2.8 barns/atom
X-ray Absorption Edge 1.195 Å1.195 ÅK
 9.535 Å9.535 ÅLI
 10.613 Å10.613 ÅLII
 10.8546 Å10.8546 ÅLIII
Electrode Potential -0.520 V-0.520 V
Electronegativity 1.811.81Pauling
Ionic Radius 0.620 Å0.620 ÅCrystal Ionic Radius for Valence +3
 0.810 Å0.810 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 2.45 g/A/h2.45 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 5050
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000175 ohm-cm0.0000175 ohm-cma-axis
Magnetic Susceptibility -3.10e-7-3.10e-7cgs/g
Critical Magnetic Field Strength, Oersted 560560Beta
 815815Delta
 950950Gamma
Critical Superconducting Temperature 5.90 - 6.20 K5.90 - 6.20 K5.9, 6.2 for Beta Ga
 7.00 K7.00 KGamma Ga
 7.85 K7.85 KDelta Ga
 6.28 K
@Pressure >=3500 MPa
6.28 K
@Pressure >=508000 psi
Ga II
 7.50 K
@Pressure >=3500 MPa
7.50 K
@Pressure >=508000 psi
Ga II′
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 80.4 J/g34.6 BTU/lb
Heat of Vaporization 3894 J/g1675 BTU/lb
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
32.2 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.330 J/g-°C0.0789 BTU/lb-°F
Thermal Conductivity 41.0 W/m-K285 BTU-in/hr-ft²-°F
Melting Point 29.78 °C85.60 °F
Boiling Point 2204 °C3999 °F
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1)  0.713
@Wavelength 589 nm
0.713
@Wavelength 589 nm
 0.756
@Wavelength 436 nm
0.756
@Wavelength 436 nm
 0.89
@Wavelength 436 nm
0.89
@Wavelength 436 nm
Liquid
 0.89
@Wavelength 589 nm
0.89
@Wavelength 589 nm
Liquid
 
Component Elements PropertiesMetricEnglishComments
Gallium, Ga 100 %100 %
 
Descriptive Properties
CAS Number7440-55-3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium, In
Gold, Au
Silver, Ag
Aluminum, Al
Chromium, Cr; Recrystallized

AMEGa00 / 38

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.