MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 3509 Phenolic, Granular, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Flock Filled

Material Notes: PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file E40654. 03509 is available in black or brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Density 1.59 g/cc0.0574 lb/in³ASTM D792
Water Absorption 0.169 %0.169 %ASTM D570
Linear Mold Shrinkage 0.00281 cm/cm0.00281 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8484ASTM D785
Tensile Strength, Ultimate 55.0 MPa7980 psiASTM D638
Elongation at Break 0.60 %0.60 %ASTM D638
Tensile Modulus 11.0 GPa1600 ksiASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 9.30 GPa1350 ksiASTM D790
Compressive Strength 194 MPa28100 psiASTM D695
Izod Impact, Notched 0.199 J/cm0.373 ft-lb/inASTM D256
Charpy Impact, Notched 0.220 J/cm²1.05 ft-lb/in²ASTM D256
Impact 117117J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.30e+12 ohm-cm3.30e+12 ohm-cmASTM D247
Dielectric Constant 4.84.8ASTM D150
Dielectric Strength 14.4 kV/mm366 kV/inStep by Step; ASTM D149
 17.4 kV/mm442 kV/inShort Time; ASTM D149
Dissipation Factor 0.02740.0274ASTM D150
Arc Resistance 172 sec172 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C
@Temperature 40.0 - 130 °C
32.2 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.470 W/m-K
@Temperature 100 °C
3.26 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 204 °C399 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 194 °C381 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 38 %38 %ASTM D2863
Shrinkage 0.086 %0.086 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
Plenco 1501 Polyester, Briquette, Transfer Molded
A. Schulman Diamond ABS 3501 Black 1302 Injection Molding Grade
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded

PLEL58 / 50629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.