MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bada BADAMID® LC70 FR HF natural white 643 PA66+PA6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Co-Polyamide injection molding grade, flame retardant without Halogens and without Phosphorus; broad processing range

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Moisture Absorption 2.60 - 3.20 %2.60 - 3.20 %50% r.h.; ISO 62
Water Absorption at Saturation 8.0 - 9.0 %8.0 - 9.0 %ISO 62
Melt Flow 160 g/10 min
@Load 5.00 kg,
Temperature 275 °C
160 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 160 MPa
@Load 36.5 kg
23200 psi
@Load 80.5 lb
ISO 2039-1
Tensile Strength at Break 85.0 MPa12300 psi5 mm/min; ISO 527-1/2
Tensile Strength, Yield 85.0 MPa12300 psi50 mm/min; ISO 527-1/2
Elongation at Break 4.0 %4.0 %5 mm/min; ISO 527-1/2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1/2
Tensile Modulus 3.70 GPa537 ksi1 mm/min; ISO 527-1/2
Izod Impact, Notched (ISO) 4.50 kJ/m²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC-62631-3-1
Surface Resistance 1.00e+9 ohm1.00e+9 ohmIEC-62631-3-2
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC-62631-2-1
Dielectric Strength 34.0 kV/mm864 kV/inIEC-60243-1
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC-62631-2-1
Comparative Tracking Index 600 V600 VIEC-60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 - 100 µm/m-°C33.3 - 55.6 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 60.0 - 120 µm/m-°C33.3 - 66.7 µin/in-°FISO 11359-2
Thermal Conductivity 0.330 W/m-K2.29 BTU-in/hr-ft²-°FTest plate 2 mm; DIN 52612-1
Melting Point 243 °C469 °F10 K/min; ISO 3146
Maximum Service Temperature, Air 200 °C392 °Fsome hours; EC-60216
 120 °C
@Time 7.20e+7 sec
248 °F
@Time 20000 hour
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-1/2
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Glow Wire Ignition Temperature  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
EC-60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
EC-60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
EC-60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
EC-60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA154 / 286987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.