MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Low Viscosity

Processing: Injection Molding

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D792
Water Absorption at Saturation <= 0.10 %<= 0.10 %ASTM D570
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inASTM D955
Melt Flow 40 - 60 g/10 min
@Load 2.16 kg,
Temperature 275 °C
40 - 60 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Hardness, Shore D 7575ASTM D2240
Tensile Strength at Break 34.0 MPa4930 psi50 mm/min; ASTM D638
Tensile Strength, Yield 30.0 MPa4350 psi50 mm/min; ASTM D638
Elongation at Break 250 %250 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 1.66 GPa241 ksi50 mm/min; ASTM D638
Flexural Strength 47.0 MPa6820 psi2.5 mm/min; ASTM D790
Flexural Modulus 1.69 GPa245 ksi2.5 mm/min; ASTM D790
Izod Impact, Notched  2.10 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
 NB
@Thickness 3.20 mm,
Temperature 23.0 °C
NB
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Coefficient of Friction, Dynamic 0.200.20vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.200.20vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.05.0CS-17 Wheel, 500 g; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+16 ohm-cm5.50e+16 ohm-cmASTM D257
Dielectric Constant 2.57
@Frequency 1e+6 Hz
2.57
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.20 mm
356 kV/in
@Thickness 0.126 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 42.0 J/g18.1 BTU/lbASTM D3418
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FASTM D696
Specific Heat Capacity 0.962 J/g-°C
@Temperature 23.0 °C
0.230 BTU/lb-°F
@Temperature 73.4 °F
ASTM C351
Thermal Conductivity 0.150 W/m-K
@Temperature 40.0 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 234 °C453 °F
Crystallization Temperature 222 °C432 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FUnannealed; ASTM D648
Brittleness Temperature <= -76.0 °C<= -105 °FProcedure A; ASTM D746
Glass Transition Temp, Tg 85.0 °C185 °FASTM E1356
Flammability, UL94 V-0V-0
Oxygen Index 52 %52 %ASTM D2863
 
Descriptive Properties
FormsPellets; Powder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Halar® 9414 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Westlake Plastics Halar® 901 ECTFE
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin

PSOL8Y6189 / 193110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.