MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
 1.24 g/cc0.0448 lb/in³Cond.; ISO 1183
Water Absorption 1.3 %1.3 %Dry; Sim. to ISO 62
Moisture Absorption 0.500 %0.500 %Dry; Sim. to ISO 62
Melt Flow >= 7.0 g/10 min>= 7.0 g/10 minASTM D1238
 7.0 g/10 min
@Load 5.00 kg,
Temperature 235 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiCond.; ISO 527-1/-2
 112 MPa16200 psiDry; ISO 527-1/-2
Tensile Strength, Yield 105 MPa15200 psiCond.; ISO 527-1/-2
 116 MPa16800 psiDry; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %Cond.; ISO 527-1/-2
 5.0 %5.0 %Dry; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %Dry; ISO 527-1/-2
 4.0 %4.0 %Cond.; ISO 527-1/-2
Tensile Modulus 6.40 GPa928 ksiCond.; ISO 527-1/-2
 6.90 GPa1000 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  7.70 J/cm²
@Temperature 23.0 °C
36.6 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
 7.90 J/cm²
@Temperature 23.0 °C
37.6 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 8.30 J/cm²
@Temperature -30.0 °C
39.5 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 8.30 J/cm²
@Temperature -30.0 °C
39.5 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmCond.; IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmCond.; IEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inDry; IEC 60243-1
 35.0 kV/mm889 kV/inCond.; IEC 60243-1
Dissipation Factor  0.0274
@Frequency 1e+6 Hz
0.0274
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.0664
@Frequency 100 Hz
0.0664
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C27.8 µin/in-°FDry; ISO 11359-1/-2
Melting Point 183 °C361 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 176 °C349 °FDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FDry; ISO 75-1/-2
Vicat Softening Point 165 °C329 °F50°C/h 50N; Dry; ISO 306
Decomposition Temperature 224 °C435 °F1% wt. loss, TGA, in nitrogen
 227 °C441 °F1% wt. loss, TGA, in air
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Yellow Card Available; Dry; IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Hold Pressure 16.0 MPa2320 psiInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® GC25T POM, 25% Glass Reinforced
Delrin Delrin® 577 BK000 POM-GF20
Arkema Rilsamid® AZM 30 O TLD PA12-GF30
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
EMS-Grivory Grilamid® LV-3H PA12-GF30

PARKF865 / 193613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.