MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubriplate 930-AA Bentone Type Multi-Purpose Grease
Categories: Fluid; Lubricant; Clay Gellant

Material Notes: Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short intervals up to 400°F / 204°C. Available in 4 NLGI densities for a wide range of applications.

Applications: High temperatures, automatic dispensers.

930 Series Greases are available in Cartridges, Tubes, Cans, Pails, 1/4 Drums & Drums.

Information provided by Lubriplate

Key Words: Part Number L0096-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Saybolt Viscosity at 100°F 750 SUS750 SUS
Kinematic Viscosity at 40°C (104°F) 135 cSt135 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 310310Unknown Amount of Work
Penetration P(60), 1/10 mm 340340Unknown Amount of Work
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 191 °C375 °F
 204 °C400 °FShort Intervals
Minimum Service Temperature, Air -17.8 °C0.000 °FApprox. Cold test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW/EP
NLGI Grade1
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WLUBR063 / 76109

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.