MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Tribocomp® PA66 LGF30 PTFE15 MoS0.5 30% long glass fiber reinforced high-flow with PTFE/MoS2
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/MoS2 Filled

Material Notes: 30% long glass fiber reinforced high-flow PA66 with a PTFE/MoS2 package

Tribocomp® PA66 LGF30 PTFE15% MoS0.5% is a 30% long glass fiber reinforced high-flow PA66 compound containing a PTFE/MoS2 package. It has been specifically designed for friction and wear applications. It can be easily be processed on most injection molding machines.

Applications: Automotive Applications; Automotive Under the Hood; Engineering Parts; Gears; Industrial Applications; Power/Other Tools

Features: Abrasion Resistant; Heat Stabilized; High Flow; High Friction; High Temperature Strength; Low Shrinkage

The value listed as Molding Shrinkage ISO 294-4, was tested in accordance with S.O.P. methods.

Injection notes: Pre-drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. At a humidity content above 0.1%, the material will begin to degrade. Recommended drying time is 4 hours at 100°C in dry-air dryer.
Processing temperatures -- Melt temperature should be kept below 300°C in order to prevent degradation. The exact setting depends from machine and mold design, but is usually within the range indicated in the Processing Information section of this TDS.
Mold temperature -- The mold temperature is a compromise between the optimum properties that can be obtained from high crystallization, and cycle time. This material can be processed at mold temperatures between 80°C and 140°C. Optimum surface quality requires a mold temperature above 120°C.
Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 15%, and only regrind of optimum quality should be used. In any case, part properties should be checked.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Moisture Absorption 1.40 %1.40 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  125 MPa
@Temperature 90.0 °C
18100 psi
@Temperature 194 °F
ISO 527-2
 200 MPa
@Temperature 23.0 °C
29000 psi
@Temperature 73.4 °F
ISO 527-2
Elongation at Break 2.7 %2.7 %ISO 527-2
Tensile Modulus  6.70 GPa
@Temperature 90.0 °C
972 ksi
@Temperature 194 °F
ISO 527-2
 10.9 GPa
@Temperature 23.0 °C
1580 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 285 MPa41300 psiISO 178
Flexural Modulus 10.6 GPa1540 ksiISO 178
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO 179
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO 179
Coefficient of Friction, Dynamic 0.230.23ASTM D1894
Coefficient of Friction, Static 0.180.18ASTM D1894
K (wear) Factor 26.2 x 10-8 mm³/N-M13.0 x 10-10 in³-min/ft-lb-hrASTM D3702
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm
@Thickness 2.00 mm
889 kV/in
@Thickness 0.0787 in
IEC 60243-1
Comparative Tracking Index 500 V500 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C10.6 µin/in-°FISO 11359-2
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 262 °C504 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 258 °C496 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 300 °C554 - 572 °F
Middle Barrel Temperature 300 °C572 °F
Front Barrel Temperature 300 °C572 °F
Nozzle Temperature 300 °C572 °F
Melt Temperature <= 300 °C<= 572 °FInjection
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 - 100 °C
@Time 14400 sec
176 - 212 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
ProcessingCompression Molding; Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4564 / 280364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.