MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastar AN004 Natural PCTA Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; PCTA Polyester Alloy; Polycyclohexylenedimethylene Terephthalate (PCT)

Material Notes: Eastar™ AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. It features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but AN004 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Its processability coupled with its outstanding chemical resistance makes it well suited for thick-wall applications.

Application/Uses:

  • Compacts
  • Cosmetic jar caps
  • Cosmetic jars
  • Cosmetics/personal care packaging
  • Fragrance caps
  • Fragrance packaging
  • Lipstick containers
  • Personal care bottles
Key Attributes:
  • Easy to extrude, cut, print, and seal
  • Effective barrier properties
  • Excellent chemical resistance
  • Excellent clarity
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Toughness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792 and ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength at Break 51.0 MPa7400 psiASTM D638
Tensile Strength, Ultimate 46.0 MPa6670 psiISO 527
Tensile Strength, Yield 47.0 MPa6820 psiISO 527 and ASTM D638
Elongation at Break 200 %200 %ISO 527
 320 %320 %ASTM D638
Elongation at Yield 4.0 %4.0 %ISO 527
 5.0 %5.0 %ASTM D638
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 69.0 MPa10000 psiASTM D790
Flexural Yield Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 1.85 GPa268 ksiISO 178
 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 0.780 J/cm1.46 ft-lb/inASTM D256
 0.480 J/cm
@Temperature -40.0 °C
0.899 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
Puncture Energy  42.0 J
@Temperature 23.0 °C
31.0 ft-lb
@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
 48.0 J
@Temperature -40.0 °C
35.4 ft-lb
@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Constant  2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D 150
 2.3
@Frequency 1000 Hz
2.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.3 kV/mm439 kV/inShort Time, 500 V/sec rate-of-rise; ASTM D 149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
High Voltage Arc-Tracking Rate, HVTR 38.0 mm/min1.50 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FASTM D 648
 
Optical PropertiesMetricEnglishComments
Haze 3.6 %3.6 %ASTM D1003
Transmission, Visible 77 %77 %Regular transmittance per ASTM D 1003
 81 %81 %Total Transmittance; ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °F
Mold Temperature 47.5 °C118 °F
Drying Temperature 95.0 °C203 °F
Dry Time 6 hour6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman DURASTAR DS1010 Natural PCTA Copolyester
Overview of materials for PCTA Polyester Alloy
Eastman Eastar BR003 Natural PCTA Copolyester
A. Schulman Diamond NPP 60-1010 PCTA Polyester Alloy
Eastman DURASTAR DS2010 Natural PCTA Copolyester

PEA020 / 35222

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.