MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 1100-8134 Polyether sulfone with carbon fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone, Carbon Fiber Reinforced

Material Notes: Properties/attributes include: High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range. Especially suitable for thin wall complex parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Superheated-steam sterilizable.

Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical engineering, aircraft- and aerospace industry. Typical uses include: High quality terminal bar, switches and plugs, relays, lamp reflectors, sterilizable medical equipment.

Processing: During processing the moisture level should not exceed 0.05%, otherwise porosity and surface defects (e.g. smearing) may occur. To avoid internal stresses, a low shear load should be used for processing. The parts may be tempered at a later stage to reduce internal stresses. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.100 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.00050 - 0.0030 cm/cm0.00050 - 0.0030 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 180 MPa26100 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Modulus of Elasticity 19.0 GPa2760 ksiISO 527-2
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Flexural Strain at Break 2.4 %2.4 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 60167
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °FContinuous; UL 746B
 200 °C392 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 340 - 360 °C644 - 680 °F
Zone 1 355 - 375 °C671 - 707 °F
Zone 2 360 - 380 °C680 - 716 °F
Zone 3 350 - 370 °C662 - 698 °F
Melt Temperature 350 °C662 °F
Mold Temperature 120 - 200 °C248 - 392 °F
Drying Temperature 150 °C
@Time 10800 - 18000 sec
302 °F
@Time 3.00 - 5.00 hour
Dehumidifying dryer
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Colorblack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1400 Polyethersulfone (PES)
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber
Lehvoss LUVOCOM® 1100-8549 Polyether sulfone with carbon fiber, PTFE, lubricant modified
Lehvoss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone with glass fiber, easy flowing, demolding aid
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE

PLUU8816 / 193775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.