MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Impact Grade, Filled

Material Notes: This Valite product has been replaced by Plenco 7697. Data provided by Plenco.

VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. It is used in automotive and oil well applications anc can be molded by compression, transfer, or injection precesses. VALITE 697-A is the same formulation as PLENCO 07697. Plenco drop ball 113g test value is 55 cm.


Plenco has discontinued their Valite product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ASTM D792
Apparent Bulk Density 0.520 g/cc0.0188 lb/in³ASTM D1895
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inPost shrinkage is 0.17% at 72hr 120°C.; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 9090ASTM D785
Tensile Strength, Ultimate 60.3 MPa8750 psiASTM D638
Elongation at Break 0.70 %0.70 %ASTM D638
Tensile Modulus 10.0 GPa1450 ksiASTM D638
Flexural Yield Strength 92.2 MPa13400 psiASTM D790
Flexural Modulus 9.10 GPa1320 ksiASTM D790
Compressive Yield Strength 227.3 MPa32970 psiASTM D695
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
Charpy Impact, Notched 0.280 J/cm²1.33 ft-lb/in²J/cm; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4.09e+12 ohm-cm4.09e+12 ohm-cmASTM D257
Dielectric Constant 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm381 kV/inShort Term per ASTM D149.
Dissipation Factor 0.036
@Frequency 1e+6 Hz
0.036
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 140 sec140 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 199 °C390 °FHeat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 206 °C403 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEO83 / 50787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.