MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Koattro PB M 0600M Polybutene Random Copolymer
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Polybutene-1 grade Koattro PB M 0600M is a random copolymer of butene-1 with high ethylene content. Koattro PB M 0600M is primarily used as a blend component in woodworking, assembly and packaging hot melt adhesive (HMA) formulations and sealant compounds. It can be used in combination with a wide variety of nonpolar resins and waxes and maintains good cohesive strength of the HMA and higher Shear Adhesion Failure Temperature (SAFT). Koattro PB M 0600M offers extended Open time, short Setting time and superior cleavage in HMA packaging applications. Koattro PB M 0600M enhances softness and flexibility and helps to reduce the amount of resin needed in HMA formulations. It is highly compatible with polypropylene.

Status: Commercial – Active

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Hot Melt Adhesives; Polymer Modifier; Sealants

Market: Compounding; Textile

Processing Method: Extrusion Coating; Melt Blown; Spunbond

Attribute: Extended Open Time; Good Adhesion; Good Thermal Stability; Short Set Time

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183-1
Brookfield Viscosity 13500 cP
@Temperature 190 °C
13500 cP
@Temperature 374 °F
ASTM D3236
Melt Flow 600 g/10 min
@Load 2.16 kg,
Temperature 190 °C
600 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.100 GPa14.5 ksiISO 178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9637 / 324572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.