MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.37 - 1.87 g/cc0.0495 - 0.0676 lb/in³Average value: 1.67 g/cc Grade Count:47
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 25.0 % Grade Count:4
Water Absorption 0.850 - 2.10 %0.850 - 2.10 %Average value: 1.32 % Grade Count:13
Moisture Absorption at Equilibrium 1.10 - 2.10 %1.10 - 2.10 %Average value: 1.53 % Grade Count:19
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 25.0 % Grade Count:5
Linear Mold Shrinkage 0.00150 - 0.0200 cm/cm0.00150 - 0.0200 in/inAverage value: 0.00550 cm/cm Grade Count:30
Linear Mold Shrinkage, Transverse 0.00300 - 0.0200 cm/cm0.00300 - 0.0200 in/inAverage value: 0.0106 cm/cm Grade Count:16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100 - 120100 - 120Average value: 116 Grade Count:9
Tensile Strength, Ultimate 55.0 - 200 MPa7980 - 29000 psiAverage value: 141 MPa Grade Count:39
 85.0 - 130 MPa
@Temperature 120 - 160 °C
12300 - 18900 psi
@Temperature 248 - 320 °F
Average value: 104 MPa Grade Count:4
Tensile Strength, Yield 45.0 - 131 MPa6530 - 19000 psiAverage value: 96.8 MPa Grade Count:7
Elongation at Break 0.600 - 50.0 %0.600 - 50.0 %Average value: 3.86 % Grade Count:43
 3.00 - 4.00 %
@Temperature 120 - 160 °C
3.00 - 4.00 %
@Temperature 248 - 320 °F
Average value: 3.25 % Grade Count:4
Elongation at Yield 3.00 - 3.80 %3.00 - 3.80 %Average value: 3.53 % Grade Count:3
Modulus of Elasticity 1.20 - 18.0 GPa174 - 2610 ksiAverage value: 10.8 GPa Grade Count:41
 6.20 - 11.0 GPa
@Temperature 120 - 160 °C
899 - 1600 ksi
@Temperature 248 - 320 °F
Average value: 8.34 GPa Grade Count:4
Flexural Yield Strength 110 - 262 MPa16000 - 38000 psiAverage value: 198 MPa Grade Count:14
Flexural Modulus 1.10 - 15.0 GPa160 - 2180 ksiAverage value: 8.90 GPa Grade Count:33
 5.00 - 10.5 GPa
@Temperature 120 - 160 °C
725 - 1520 ksi
@Temperature 248 - 320 °F
Average value: 7.38 GPa Grade Count:4
Izod Impact, Notched 0.427 - 1.33 J/cm0.800 - 2.50 ft-lb/inAverage value: 0.759 J/cm Grade Count:14
Izod Impact, Unnotched 4.27 - 7.47 J/cm8.00 - 14.0 ft-lb/inAverage value: 5.81 J/cm Grade Count:9
Izod Impact, Notched (ISO) 2.00 - 15.0 kJ/m²0.952 - 7.14 ft-lb/in²Average value: 11.0 kJ/m² Grade Count:16
 5.00 - 15.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.38 - 7.14 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 10.4 kJ/m² Grade Count:15
Charpy Impact Unnotched 1.00 J/cm² - NB4.76 ft-lb/in² - NBAverage value: 5.06 J/cm² Grade Count:26
 1.00 - 9.50 J/cm²
@Temperature -30.0 - -30.0 °C
4.76 - 45.2 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.74 J/cm² Grade Count:19
Charpy Impact, Notched 0.200 - 1.50 J/cm²0.952 - 7.14 ft-lb/in²Average value: 0.991 J/cm² Grade Count:31
 0.160 - 1.40 J/cm²
@Temperature -30.0 - -30.0 °C
0.761 - 6.66 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.999 J/cm² Grade Count:25
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+8 - 1.00e+15 ohm-cm1.00e+8 - 1.00e+15 ohm-cmAverage value: 1.55e+14 ohm-cm Grade Count:34
Dielectric Strength 20.0 - 30.0 kV/mm508 - 762 kV/inAverage value: 25.4 kV/mm Grade Count:31
Comparative Tracking Index 175 - 600 V175 - 600 VAverage value: 316 V Grade Count:19
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 - 90.0 µm/m-°C9.44 - 50.0 µin/in-°FAverage value: 29.0 µm/m-°C Grade Count:26
CTE, linear, Transverse to Flow 25.0 - 90.0 µm/m-°C13.9 - 50.0 µin/in-°FAverage value: 56.9 µm/m-°C Grade Count:22
Melting Point 295 °C563 °FAverage value: 295 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 123 - 290 °C254 - 554 °FAverage value: 276 °C Grade Count:32
UL RTI, Electrical 130 - 140 °C266 - 284 °FAverage value: 139 °C Grade Count:7
Flammability, UL94 V-0V-0Grade Count:35
Oxygen Index 37.0 %37.0 %Average value: 37.0 % Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 293 - 321 °C560 - 610 °FAverage value: 307 °C Grade Count:4
Melt Temperature 293 - 327 °C560 - 620 °FAverage value: 310 °C Grade Count:5
Mold Temperature 79.4 - 149 °C175 - 300 °FAverage value: 114 °C Grade Count:9
Drying Temperature 121 °C250 °FAverage value: 121 °C Grade Count:5
Moisture Content 0.0500 %0.0500 %Average value: 0.0500 % Grade Count:5
Dew Point -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 46, Glass Fiber Reinforced
Overview of materials for Nylon 46, Unreinforced
Overview of materials for Nylon 6, Impact Grade
Overview of materials for Nylon 6, Heat Stabilized
Overview of materials for Nylon 6, Unreinforced

O2392 / 77959

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.