MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Formic Acid - 85%
Categories: Fluid; Solvent

Material Notes: Formula: CH2O2

CAS: 64-18-6

Description: Formic Acid 85% is a colorless to yellowish liquid, with a pungent odor. It is miscible with water and other organic substances in all proportions.

Synonyms: Methanoic Acid, Formylic Acid

Applications: Intermediate used in the production of Crop protection agents, Dyes, Flue gas, Industrial chemicals, Pesticides, PH control/neutralization, Pharmaceuticals, Plastics, Rubber industry and Textile industry; Also used as a Initial product for chemical synthesis, Silage additive and Solvent

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.195 g/cc0.04317 lb/in³
Molecular Weight 46 g/mol46 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -50.8 °C-59.4 °F
Boiling Point 107.3 °C225.1 °F
Flash Point 65.0 °C149 °F
Ignition Temperature 500 °C932 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 14 - 16 %14 - 16 %DIN 51 777
 
Descriptive Properties
Color<50APHA, DIN EN 1557
CompositionAcetic acid<50 ppm, ISO 731/VII
 Non-volatile matter<50 ppm, AAS/AES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Formic Acid - 99-100%
BASF Formic Acid - 95%
Formic acid (Methanoic acid), HCOOH

PBASG0963 / 132596

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.