MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Mica Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inMD; ASTM D955
Melt Flow 12 g/10 min12 g/10 minASTM D1238
Ash 10 %10 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5353ASTM D785
Tensile Strength at Break 16.0 MPa2320 psiASTM D638
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638
Elongation at Break 26 %26 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 1.500 GPa217.5 ksiASTM D638
Flexural Strength 27.0 MPa3920 psiASTM D790
Flexural Modulus 1.350 GPa195.8 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced
Aclo Accutech Polypropylene Copolymer CP0436T10L Talc Reinforced
Aclo Accutech Polypropylene Homopolymer HP0334T10L Talc Reinforced
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced
Crystex Composites Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite

PACLO187 / 22442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.