MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Hexcel® HiMax™ FAHM106 [GE/AHM, 340, -45/+45, 150PV] Glass Fiber Biaxial +/- 45 (Hybrid) Fabric
Categories: Ceramic; Glass; Glass Fiber; Polymer; Thermoset; Aramid

Material Notes: Stitching Fiber
Stitching Thread: Texturized Polyester
Stitch DTex: 78
Stitch Gauge: 3.0 gg
Stitch Length: 2.12 mm
Stitch Type: Pillar
Stitch Weight: 4 gsm

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Fabric Weight490 g/m2
Ply construction150 g/m2CSM, Ply Weight
 300 texCSM, Fiber Tex
 8 ggCSM, Gauge
 E-GlassCSM, Fiber Specification
Ply construction 45°1.75 ggAramid, Gauge
 134 g/m2E-Glass, Ply Weight
 300 texE-Glass, Fiber Tex
 33 g/m2Aramid, Ply Weight
 340 texAramid, Fiber Tex
 8 ggE-Glass, Gauge
 AramidAramid, Fiber Specification
 E-GlassE-Glass, Fiber Specification
Ply construction -45°1.75 ggAramid, Gauge
 134 g/m2E-Glass, Ply Weight
 300 texE-Glass, Fiber Tex
 33 g/m2Aramid, Ply Weight
 340 texAramid, Fiber Tex
 8 ggE-Glass, Gauge
 AramidAramid, Fiber Specification
 E-GlassE-Glass, Fiber Specification

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHECF9054 / 322210

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.