MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecamid® 6/12 Nylon (PA612)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.

Information Provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Water Absorption 0.25 %0.25 %at 24 hours; ASTM D570
Water Absorption at Saturation 3.0 %3.0 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength, Yield 55.2 MPa8000 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Tensile Modulus 2.07 GPa300 ksiASTM D638
Flexural Modulus 1.90 GPa275 ksiASTM D790
Compressive Strength 16.5 MPa2400 psiASTM D695
Izod Impact, Notched 0.481 J/cm0.900 ft-lb/inASTM D256
Coefficient of Friction, Static 0.310.31ASTM D3702
K (wear) Factor 383 x 10-8 mm³/N-M190 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150
 4.0
@Frequency 60 Hz
4.0
@Frequency 60 Hz
ASTM D150
Dissipation Factor 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.88 J/g-°C0.450 BTU/lb-°F
Melting Point 217 °C422 °FASTM D2133
Deflection Temperature at 1.8 MPa (264 psi) 61.1 °C142 °FASTM D648
Flammability, UL94 HB
@Thickness 0.860 mm
HB
@Thickness 0.0339 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecamid® 6/6 Nylon (PA66)
Arkema Rilsamid® AECHVO TL PA12
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)
Overview of materials for Nylon 12
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6

PENS72 / 35995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.