MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resistance; widely used for auto parts, quick connectors, housing et al;

Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/innormal; ISO 294-4,2577
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inISO 294-4,2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 137 MPa19900 psiISO527-2/1A
Elongation at Break 5.0 %5.0 %ISO 527-2/1A
Tensile Modulus 7.80 GPa1130 ksiISO 527-1/-2
Charpy Impact Unnotched  9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmISO 60695
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 213 °C415 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75-1/2
Vicat Softening Point 210 °C410 °FISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC60695
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 290 °C482 - 554 °F
Mold Temperature 60.0 - 110 °C140 - 230 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Injection Pressure 70.0 - 130 MPa10200 - 18900 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PA6-GF60-01 Nylon 6, 60% Glass Reinforced
Arkema Rilsamid® DZM 30 BLACK TL PA612-GF30
Celanese Zytel® 77G33L BK031 PA612-GF33
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated
EMS-Grivory Grilamid® XE 4106 black 9992 PA612-GF30

PHIPRO10 / 106825

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.