MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Mobil Centaur Moly 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly  products represents a significant advance in grease formulation technology. Unlike conventional soap-base thickeners (i.e. lithium, aluminium, and calcium soaps), the calcium sulfonate thickener does much more than simply impart consistency. It imparts excellent corrosion and water-resistance properties to the grease and has inherent extreme-pressure protection properties that enhance load-carrying ability. Further, the EP properties derived from the calcium thickener also have inherently better thermal stability than those from conventional Sulphur/Phosphorus EP additives. Fortified with molybdenum disulphide to complement its robust extreme-pressure additive system, Mobil Centaur Moly  is particularly well suited to meet the demanding lubrication requirements of heavy-duty truck chassis, construction and mining equipment, and heavily load industrial bearings. Mobil Centaur Moly  also provides outstanding resistance against the effects of water washout, water spray-off and corrosion.

Mobil Centaur Moly  products are highly recommended for heavily loaded applications or environments highly contaminated with water. Specific examples of such applications include: Heavy-duty trucks, including chassis, spring shackles, king pins, tie rods, u-joints, hinge and bucket pins and fifth wheels; Mining and construction equipment; Marine equipment; Highly loaded industrial bearings

Key Words: NLGI Grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 320 cSt320 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 500 kg1100 lb (mass)ASTM D2596
Four Ball Wear 0.380 mm0.0150 in40 kg, 1200 rpm; ASTM D2266
Penetration >= 265>= 265Worked, 25°C; ASTM D217
Timken Test 27200 g60.0 lb
 
Thermal PropertiesMetricEnglishComments
Dropping Point 280 °C536 °FASTM D2265
 
Descriptive Properties
Colorgrey
Soap/Thickener Typecalcium sulfonate
Water Spray Resistance, ASTM D4049, % Spray-off20
Water Washout, ASTM D1264, wt%1@ 79°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Sand Cast and Heat Treated
Overview of materials for Low Carbon Steel
Overview of materials for Cobalt Alloy

WEXXON370 / 75795

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.