MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bromine, Br2
Categories: Fluid; Pure Element

Material Notes: CAS Number: 7726-95-6

Physical Form: Red Liquid

Key Words: Bromine, Br2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.1028 g/cc0.11210 lb/in³
Viscosity 0.996 cP
@Temperature 20.0 °C
0.996 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 159.808 g/mol159.808 g/mol
Vapor Pressure 0.231099 bar
@Temperature 20.0 °C
173.339 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 79.90479.9041995
Atomic Number 3535
X-ray Absorption Edge 0.91994 Å0.91994 ÅK
 6.925 Å6.925 ÅLI
 7.7523 Å7.7523 ÅLII
 7.9871 Å7.9871 ÅLIII
Critical Pressure 103.400 bar77556.4 torr
Critical Temperature 315 °C599 °F
Critical Density 1.258 g/cc0.04545 lb/in³
Critical Molar Volume 127 cm³/mol7.75 in³/mol
Electronegativity 2.962.96Pauling
Ionic Radius 0.390 Å0.390 ÅCrystal Ionic Radius for Valence +7
 0.470 Å0.470 ÅCrystal Ionic Radius for Valence +5
 1.96 Å1.96 ÅCrystal Ionic Radius for Valence -1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.15
@Temperature 20.0 °C
3.15
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 65.83 J/g28.32 BTU/lb
Heat of Vaporization 187.5 J/g80.65 BTU/lbAt Boiling Point
 193.4 J/g
@Temperature 25.0 °C
83.20 BTU/lb
@Temperature 77.0 °F
Specific Heat Capacity 0.226 J/g-°C0.0540 BTU/lb-°F
 0.4737 J/g-°C0.1132 BTU/lb-°FLiquid
 0.229 J/g-°C
@Temperature 25.0 °C
0.0547 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.123 W/m-K
@Temperature 20.0 °C
0.854 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -7.20 °C19.0 °F
Boiling Point 58.8 °C138 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molLiquid
 30.9 kJ/mol30.9 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.659
@Temperature 15.0 °C,
Wavelength 589 nm
1.659
@Temperature 59.0 °F,
Wavelength 589 nm
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 100 %100 %
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8441
Antoine's Vapor Pressure B Parameter2582.32
Antoine's Vapor Pressure C Parameter-51.56
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
AppearanceRed Liquid
CAS Number7726-95-6
Critical Compressibility (Zc)0.27
Dipole moment (p/C.m)6.671E-29
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A387.82
Dynamic Viscosity Parameter B292.79
Molar Heat Capacity (298K)36.521 J/mol-K
Molar Heat Capacity of Vapor a Parameter33.836
Molar Heat Capacity of Vapor b Parameter0.0112
Molar Heat Capacity of Vapor c Parameter-1.191E-05
Molar Heat Capacity of Vapor d Parameter4.531E-09
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
SolubilitySoluble in H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fluorine, F2
Argon, Ar
Chlorine, Cl2
Helium, He
Neon, Ne

AMEBr / 15

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.