MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Surlyn® SURSG201UG  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and provides improved scratch and abrasion resistance. Surlyn Reflections® SG201UG is an excellent, lower cost, more environmentally friendly alternative to painting.

Information provided by DuPont™

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.043 g/cc0.03768 lb/in³ASTM D792-ISO 1183
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.8 MPa6500 psiASTM D638 ISO 527-2
Elongation at Break >= 200 %>= 200 %ASTM D638 ISO 527-2
Flexural Modulus 1.00 GPa145 ksiASTM D790
Izod Impact, Notched 2.67 J/cm5.00 ft-lb/inLow Temp; ASTM D256
 6.41 J/cm12.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 93.6 µm/m-°C
@Temperature 20.0 °C
52.0 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C136 °FASTM D648
Vicat Softening Point 190 °C374 °FASTM D1525, ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1650SB
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Surlyn® 1702SBR
Dow Surlyn® SG201U NC010 Supergloss Molding Alloy
Dow Surlyn® 8945 Thermoplastic Ionomer Resin

PDUP956 / 33523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.