MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 4504 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Cellulose Filled

Material Notes: Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical properties, it has found use in a wide variety of wiring device applications. It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³ASTM D1895
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Water Absorption 0.224 %0.224 %ASTM D570
Linear Mold Shrinkage 0.0069 cm/cm0.0069 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7878ASTM D785
Tensile Strength, Ultimate 52.0 MPa7540 psiASTM D638
Elongation at Break 0.70 %0.70 %ASTM D638
Tensile Modulus 9.90 GPa1440 ksiASTM D638
Flexural Strength 79.0 MPa11500 psiASTM D790
Flexural Modulus 8.90 GPa1290 ksiASTM D790
Compressive Strength 173 MPa25100 psiASTM D695
Izod Impact, Notched 0.171 J/cm0.320 ft-lb/inASTM D256
Charpy Impact, Notched 0.168 J/cm²0.800 ft-lb/in²ASTM D256
Impact 9999J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+11 ohm-cm3.00e+11 ohm-cmASTM D247
Dielectric Constant 5.65.6ASTM D150
Dielectric Strength 10.5 kV/mm267 kV/inShort Time; ASTM D149
Dissipation Factor 0.0740.074ASTM D150
Arc Resistance 177 sec177 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 196 °C385 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 179 °C354 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.299 %0.299 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2369 Phenolic, Granular, Compression Molded
Plenco 2311 Phenolic, Granular, Transfer Molded
Plenco 2311 Phenolic, Granular, Injection Molded
Plenco 2308 Phenolic, Granular, Transfer Molded
Plenco 2308 Phenolic, Granular, Injection Molded

PLEL89n / 50664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.