MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PIPG 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: PIPG (recycled Post-Industrial PET-G) filament is strong & flexible, odor neutral and easy to print on most of the conventional desktop printers with a heated build plate. Very low shrinkage and almost no warping make PIPG an excellent material which combines the advantages of both PLA and ABS.

Features:

  • Post Industrial Recycled Grade
  • Strong & Flexible
  • Easy to Print
  • Limited Smell
  • Almost no “Warping”
Colors: PET-G is available from stock in 19 colors. Other colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccISO 1183
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 7.3 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.3 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psiISO 527
Elongation at Break 61 %61 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 2.05 GPa297 ksi(E); ISO 527
Charpy Impact, Notched 0.490 J/cm²2.33 ft-lb/in²ISO 179
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 240 °C446 - 464 °FPrinting Temperature
 
Descriptive Properties
Bed Temp=70°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9835 / 301060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.