MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ABM Composite ArcBiox™ MFA20-B2000 PLA-based Compound
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: PLA-based compound with mineral reinforcement for injection moulding

Features:

  • Cold mould and fast cycle
  • Good temperature resistance
  • Industrial compostable according to EN13432
  • Food approved
  • Bio-based content 75%
  • Reusable cups, pots, plates etc
  • Cosmetics
  • Good alternative for PP materials
Applications:
  • Reusable cups, pots, plates etc
  • Cosmetics
  • Good alternative for PP materials

Information provided by Arctic Biomaterials Oy Composite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inISO 294-4
Melt Flow 29 g/10 min
@Load 5.00 kg,
Temperature 200 °C
29 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 MPa18100 psiHB 358; ISO 2039-1
Tensile Strength at Break 28.0 MPa4060 psiISO 527
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Break 10 %10 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 4.50 GPa653 ksiISO 527
Flexural Strength 79.0 MPa11500 psiISO 178
Flexural Modulus 3.98 GPa577 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 36.0 kJ/m²17.1 ft-lb/in²ISO 180/U
Charpy Impact Unnotched 4.40 J/cm²20.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FISO 75
Vicat Softening Point 77.0 °C171 °F50N, 50 °C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 50.0 °C86.0 - 122 °FFeed Throat
 180 - 200 °C356 - 392 °FCompression Section
 180 - 200 °C356 - 392 °FMetering Section
Feed Temperature 170 - 190 °C338 - 374 °F
Nozzle Temperature 180 - 200 °C356 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 °C176 °F
Dry Time 5.00 hour5.00 hour
Dew Point -40.0 °C-40.0 °F
Back Pressure 1.00 - 2.00 MPa145 - 290 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PABMC002 / 249361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.