MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Used in bearing applications. ZA-27 has a higher bearing load capacity than bronze bearing alloys, although its environment (both temperature and corrosive) is more limited.

Key Words: Zinc Foundry Alloy; UNS Z35841 (Castings); UNS Z35840 (Ingot)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.02 g/cc0.181 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 424 MPa61500 psi
Elongation at Break 2.0 %2.0 %in 5 cm
Modulus of Elasticity 77.9 GPa11300 ksi
Fatigue Strength 117 MPa
@# of Cycles 5.00e+8
17000 psi
@# of Cycles 5.00e+8
Reverse Bending
Coefficient of Friction 0.030 - 0.0700.030 - 0.070
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000580 ohm-cm0.00000580 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 128 J/g55.1 BTU/lb
CTE, linear 26.0 µm/m-°C
@Temperature 20.0 - 200 °C
14.4 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°F
Thermal Conductivity 125 W/m-K868 BTU-in/hr-ft²-°F
Melting Point 376 - 484 °C709 - 903 °F
Solidus 376 °C709 °F
Liquidus 484 °C903 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 515 - 545 °C959 - 1010 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 25 - 28 %25 - 28 %Addition, Casting
 25.5 - 28 %25.5 - 28 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Copper, Cu 2.0 - 2.5 %2.0 - 2.5 %Addition, Casting
 2.0 - 2.5 %2.0 - 2.5 %Addition, Ingot form
Iron, Fe <= 0.072 %<= 0.072 %Impurity, Ingot form
 <= 0.075 %<= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Magnesium, Mg 0.010 - 0.020 %0.010 - 0.020 %Addition, Casting
 0.012 - 0.020 %0.012 - 0.020 %Addition, Ingot form
Tin, Sn <= 0.0020 %<= 0.0020 %Impurity, Ingot form
 <= 0.0030 %<= 0.0030 %Impurity, Casting
Zinc, Zn 69.396 - 72.488 %69.396 - 72.488 %As balance; Ingot per ASTM B 669
 69.39 - 72.99 %69.39 - 72.99 %As balance; Castings per ASTM B 791

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Permanent Mold Cast
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Sand Cast
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Sand Cast and Heat Treated
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast

MZN27D / 14523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.