MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 00757 Melamine-Phenolic, Granular, Injection Molded  (discontinued **)
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00757 is available only in brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.610 g/cc0.0220 lb/in³ASTM D1895
Density 1.70 g/cc0.0614 lb/in³ASTM D792
Water Absorption 0.285 %0.285 %ASTM D570
Linear Mold Shrinkage 0.0057 cm/cm0.0057 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 6767ASTM D785
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM D638
Elongation at Break 0.71 %0.71 %ASTM D638
Tensile Modulus 11.8 GPa1710 ksiASTM D638
Flexural Strength 90.0 MPa13100 psiASTM D790
Flexural Modulus 9.90 GPa1440 ksiASTM D790
Compressive Strength 142 MPa20600 psiASTM D695
Izod Impact, Notched 0.205 J/cm0.384 ft-lb/inASTM D256
Charpy Impact, Notched 0.217 J/cm²1.03 ft-lb/in²ASTM D256
Impact 132132J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.30e+11 ohm-cm6.30e+11 ohm-cmASTM D247
Dielectric Constant 7.67.6ASTM D150
Dielectric Strength 5.50 kV/mm140 kV/inStep by Step; ASTM D149
 7.80 kV/mm198 kV/inShort Time; ASTM D149
Dissipation Factor 0.1140.114ASTM D150
Arc Resistance 180 sec180 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.610 W/m-K
@Temperature 100 °C
4.23 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 144 °C291 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
Oxygen Index 36 %36 %ASTM D2863
Shrinkage 0.95 %0.95 %240 hr, 105ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded
Raschig Group MELOPAS® 2010 MF Melamine
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded
DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)

PLEL09 / 50577

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.