MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americas Styrenics STYRON® EA3400 High Heat Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Product Characteristics
  • Less than 300 parts per million residual volatiles with minimal taste and odor transfer
  • Excellent clarity and color
  • Good toughness
  • Food Contact Compliant

Typical Applications

  • Cap layers in co-extrusion applications
  • Blends with SB copolymer
  • Injection molded medical devices
  • Thick wall injection molded glasses

Information provided by AmericasStyrenics LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 108108ASTM D785
Tensile Strength at Break 46.2 MPa6700 psiASTM D638
Tensile Strength 46.2 MPa6700 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 3.21 GPa465 ksiASTM D638
Flexural Strength 58.6 MPa8500 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C192 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D648
Vicat Softening Point 98.9 °C210 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 213 - 243 °C415 - 469 °FInjection Molding
Zone 1 177 - 193 °C351 - 379 °FExtrusion Molding
 218 - 249 °C424 - 480 °FInjection Molding
Zone 2 182 - 204 °C360 - 399 °FExtrusion Molding
 218 - 249 °C424 - 480 °FInjection Molding
Zone 3 188 - 210 °C370 - 410 °FExtrusion Molding
 199 - 213 °C390 - 415 °FInjection Molding
Zone 4 199 - 216 °C390 - 421 °FExtrusion Molding
Zone 5 204 - 221 °C399 - 430 °FExtrusion Molding
Die Temperature 199 - 232 °C390 - 450 °FExtrusion Molding
Melt Temperature 193 - 232 °C379 - 450 °FExtrusion Molding
Back Pressure 0.172 - 1.21 MPa25.0 - 175 psiInjection Molding
 
Descriptive Properties
Head Pressure10-21 MPa
Melt Pump, Adapter, Pipes, Screen Changer193-232°C
Polish Rolls66-104°C
Zone # 6204-221°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAMERI917b / 323907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.