MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Mocom (ALBIS) ALCOM® TCD PA66 5050 14016 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Base Polymer: Polyamide 66

Filler/Additive System: Special filler

Special Features: Thermal conductive, electrically insulating, heat ageing stabilization

Market Segment: Automotive, Machinery, Electrical and Electronic, Lighting

Application Area: Radiator systems, cooling system

Typical Applications: Housings, functional components, plugs/connectors, lamp sockets

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Time 86400 sec
0.0030 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Elongation at Break 1.0 %1.0 %ISO 527
Tensile Modulus 9.80 GPa1420 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN EN 62631-3-2
Dielectric Strength 54.0 kV/mm1370 kV/inIEC 20243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.60 J/g-°C0.382 BTU/lb-°F
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°Fthrough-plane; ASTM E 1461
 2.30 W/m-K16.0 BTU-in/hr-ft²-°FISO 22007-2
 5.00 W/m-K34.7 BTU-in/hr-ft²-°Fin-plane; ASTM E 1461
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Flammability Index 850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 320 °C572 - 608 °FInjection molding
Mold Temperature >= 100 °C>= 212 °FInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8203 / 242262

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.