MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KEP Kepital® FG2015 Acetal Copolymer, 15% Glass Fiber
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 20% Glass Fiber Reinforced

Material Notes: 15% glass fiber filled medium viscosity grade good for general injection molding. FG2015 is good for parts requiring high stiffness, strength, creep resistance, and HDT.

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %ISO 62
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 120 MPa17400 psi50 mm/min; ISO 527
Elongation at Break 3.6 %3.6 %50 mm/min; ISO 527
Flexural Strength 175 MPa25400 psiISO 178
Flexural Modulus 5.20 GPa754 ksiISO 178
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°FISO 11359
Melting Point 165 °C329 °FISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KEP Kepital® F20-03 Acetal Copolymer, Medium viscosity
KEP Kepital® FG2025 Acetal Copolymer, 25% Glass Fiber
Overview of materials for Acetal Copolymer, Unreinforced
KEP Kepital® FG1025 Acetal Copolymer, 25% Glass Fiber
KEP Kepital® FB2030 Acetal Copolymer, Glass Bead

PKEP9901 / 185577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.