MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Stainless Steel Fiber, 16% Filler by Weight

Features: Flame Retardant and Electromagnetic Shielding (EMI)

Appearance: Black

TPCI# 7965121

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.17 mm
0.0060 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.6 MPa6900 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 81.4 MPa11800 psiASTM D790
Flexural Modulus 6.21 GPa900 ksiASTM D790
Izod Impact, Notched 0.374 J/cm
@Thickness 3.17 mm
0.700 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 1.60 J/cm
@Thickness 3.17 mm
3.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.0 - 1000 ohm-cm1.0 - 1000 ohm-cmASTM D257
Surface Resistance 1.0 - 1000 ohm1.0 - 1000 ohmASTM D257
Static Decay <= 0.10 sec<= 0.10 secFTMS 101B
Shielding Effectiveness 55 dB55 dBASTM D4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C285 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTPC0961 / 136899

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.