MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® RS 1395 45% Mineral Reinforced, Radiation Crosslinkable PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:
  • high thermostability
  • high stiffness
  • low water absorption resulting in high dimensional stability
  • high hardness
  • good strength
  • good sliding friction behavior, low abrasion
  • good creep behavior
  • good electrical properties
  • good chemical resistance
  • good weathering resistance
  • good processability
  • no tendency to form stress cracks

Specific Notes for this Material: Crosslinkable with heat or radiation, with flame retardant, very fine filler.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 250 °C
22 g/10 min
@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 7.20 GPa1040 ksi
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 225 V225 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 345 °C653 °FShort-term heat resistance depending on the radiation dose (300 kGy), measured at 3.2 mm UL test bars.
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FISO 75-2
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled

PHUMA42 / 47556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.