MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness
Categories: Other Engineering Material; Composite Fibers; Polymer; Film; Thermoset; Aramid

Material Notes: Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand-wound motors and for linear wrapping of wire, but is also used where its specific characteristics are desirable, such as folded or punched parts. Nomex® Type 414 is also used in fluid filled transformers due to its improved impregnability compared to Type 410.

General NOMEX Information: Nomex® is a family of aromatic polyamide (aramid) fibers. This family consists of staple fibers, continuous filament yarns, paper, and spunlaced fabrics. The paper is produced from two forms of the aramid polymer. Small fibrous binder particles (fibrids) derived directly from the polymer under high shear conditions are mixed with short fibers (floc) which are cut to length from a fiber filament. The floc and fibrids are combined in a water based slurry from which a continuous sheet is produced on a specialized papermaking machine. This initial paper (as in Type 411) is low density and has poor properties. Subsequent densification and internal bonding is achieved by high temperature calendaring. The resulting paper is mechanically strong and has good electrical properties. Some uses for paper product include insulation in electric motors and transformers, wire wrapping, and honeycombed strength members in many aircraft. Nomex® brand fibers are inherently flame resistant: the flame resistance is a polymer property and does not diminish with the life of the fiber.

Nomex® meta-aramid, poly(meta-phenyleneisophthalamide), is prepared from meta-phenylenediamine and isophthaloyl chloride in an amide solvent. It is a long chain polyamide in which at least 85% of the amide linkages are attached directly to two aromatic rings. The meta oriented phenylene forms bends in the polymer chain, reducing chain rigidity as compared to the para orientation in the chemically similar Kevlar® chain. This flexible polymer chain gives Nomex® more textile-like qualities while retaining high temperature properties similar to Kevlar®.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.940 g/cc0.0340 lb/in³
Density 0.940 g/cc0.0340 lb/in³
Thickness 178 microns7.00 milNominal
 188 microns7.40 milTypical; ASTM D374
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 13.1 %13.1 %ASTM D828
Film Elongation at Break, TD 15.9 %15.9 %ASTM D828
Flex Crack Resistance 86008600Cycles of Fold Endurance; ASTM D2176
Tear Strength, Total 24.0 N5.40 lb (f)Initial in TD; ASTM D1004
 55.0 N12.4 lb (f)Initial in MD; ASTM D1004
Film Tensile Strength at Break, MD 91.5 MPa13300 psiCalculated from mfr's report of 172 N/cm per ASTM D828 and the typical thickness
Film Tensile Strength at Break, TD 42.0 MPa6090 psiCalculated from mfr's report of 79 N/cm per ASTM D828 and the typical thickness
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm50% RH; tested on 10 mil thickness sample; ASTM D257
Dielectric Constant  2.5
@Frequency 60 Hz
2.5
@Frequency 60 Hz
ASTM D150
 2.5
@Frequency 1000 Hz
2.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm762 kV/inAC Rapid Rise; ASTM D149
 51.0 kV/mm1300 kV/inFull-wave Impulse; ASTM D3426
Dissipation Factor 0.0080
@Frequency 60 Hz
0.0080
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °FElectrical insulation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness

PDUNOMP18 / 33444

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.