MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 384 HEC Polycarbonate (PC), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, NCG Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D 792
Filler Content 25 %25 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0010 cm/cm
@Thickness 3.17 mm
0.00050 - 0.0010 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 103 MPa15000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %ASTM D 638
Tensile Modulus 10.3 GPa1500 ksiASTM D 638
Flexural Strength 165 MPa24000 psiASTM D 790
Flexural Modulus 10.3 GPa1500 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.17 mm
1.00 ft-lb/in
@Thickness 0.125 in
D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohm<= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohm<= 1000 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 2582 C FR  Polycarbonate/ABS Alloy (PC/ABS) Shielding - Nickel-Coated Carbon Fiber 15% - Flame Retardant
RTP Company EMI 2581.2 FR  Polycarbonate/ABS Alloy (PC/ABS) Shielding - Nickel-Coated Carbon Fiber 12% - Flame Retardant
RTP Company EMI 2563 FR Polycarbonate/ABS Alloy (PC/ABS) Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 2562 Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

PQZWA13352 / 90767

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.