MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Oxford Polymers PEI 10GF-Natural PEI, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 10% Glass Fiber

Material Notes: Product Description: Glass Fiber (10% Reinforced), Polyetherimide injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Release Agents

Special Characteristics: Easy flow

Information provided by Oxford Polymers

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Water Absorption at Saturation 0.25 %0.25 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 3.17 mm
0.0050 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 114 MPa16600 psiASTM D638
Elongation at Break 5.8 %5.8 %ASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
Flexural Modulus 4.48 GPa650 ksiASTM D790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.17 mm
1.10 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 343 °C650 °F
Middle Barrel Temperature 349 °C660 °F
Front Barrel Temperature 354 °C670 °F
Nozzle Temperature 357 °C675 °F
Melt Temperature 352 °C665 °F
Mold Temperature 135 °C275 °F
Drying Temperature <= 149 °C<= 300 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxford Polymers 20GF 20% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Overview of materials for Polyetherimide (PEI)

POXF019 / 178449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.