MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Encom Polymers EnCounter 11IML PBT Alloy, Extra Tough, Lubricated
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection Molding

Applications: Good Chemical Resistance, High Gloss, Fast Cycle and Good Flow

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
@Thickness 3.20 mm
0.019 - 0.023 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa5370 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Strength 50.0 MPa7250 psiASTM D790
Flexural Modulus 1.552 GPa225.1 ksiASTM D790
Izod Impact, Notched 5.87 J/cm11.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C250 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C120 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 238 - 254 °C460 - 490 °F
Middle Barrel Temperature 238 - 254 °C460 - 490 °F
Front Barrel Temperature 243 - 260 °C470 - 500 °F
Nozzle Temperature 238 - 254 °C460 - 490 °F
Melt Temperature 243 - 260 °C470 - 500 °F
Mold Temperature 48.9 - 76.7 °C120 - 170 °F
Drying Temperature 121 °C250 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour
 <= 8.00 hour<= 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM085 / 266099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.