MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exceed™ 3512CB Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and puncture. These superior strength properties, along with excellent heat sealing and hot tack performance, make this a versatile packaging resin.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Cast Film
  • Food Packaging
  • Form Fill and Seal Packaging
  • Lamination Film
  • Multilayer Packaging Film
  • Packaging Fims
  • Personal Care
  • Premium Trash Bags
  • Stand Up Pouches
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.912 g/cc0.0329 lb/in³ASTM D1505
Thickness 20.3 microns0.800 mil
Melt Flow 3.5 g/10 min3.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 7.52 MPa1090 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 5.72 MPa830 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 410 %410 %ASTM D882
Film Elongation at Break, TD 735 %735 %ASTM D882
Puncture Energy 4.64 J3.42 ft-lbExxon Mobil Method
Elmendorf Tear Strength MD 120 g120 gASTM D1922
Elmendorf Tear Strength TD 520 g520 gASTM D1922
Elmendorf Tear Strength, MD 5.91 g/micron150 g/milASTM D1922
Elmendorf Tear Strength, TD 25.6 g/micron650 g/milASTM D1922
Dart Drop 8.366 g/micron212.5 g/milASTM D1709
Dart Drop Test 170 g0.375 lbASTM D1709
Film Tensile Strength at Break, MD 76.60 MPa11110 psiASTM D882
Film Tensile Strength at Break, TD 49.2 MPa7140 psiASTM D882
1% Secant Modulus, MD 80.53 MPa11680 psiASTM D882
1% Secant Modulus, TD 105.6 MPa15320 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 99.0 °C210 °FExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 1.6 %1.6 %ASTM D1003
Gloss 90 %90 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
Dow HDPE 10462N High Density Polyethylene
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Data
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade
ExxonMobil Exceed™ 1012CA Film Resin

PEXB126 / 37431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.