MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.775 - 1.28 g/cc0.0280 - 0.0462 lb/in³Average value: 1.05 g/cc Grade Count:73
Water Absorption 0.270 - 0.340 %0.270 - 0.340 %Average value: 0.302 % Grade Count:5
Moisture Absorption at Equilibrium 0.270 - 0.310 %0.270 - 0.310 %Average value: 0.290 % Grade Count:7
Linear Mold Shrinkage 0.000400 - 0.00700 cm/cm0.000400 - 0.00700 in/inAverage value: 0.00565 cm/cm Grade Count:37
Melt Flow 1.20 - 2.60 g/10 min1.20 - 2.60 g/10 minAverage value: 1.93 g/10 min Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80.0 - 10580.0 - 105Average value: 97.1 Grade Count:35
Tensile Strength, Ultimate 15.9 - 42.0 MPa2310 - 6090 psiAverage value: 34.3 MPa Grade Count:41
Tensile Strength, Yield 28.8 - 42.7 MPa4180 - 6200 psiAverage value: 36.6 MPa Grade Count:35
Elongation at Break 7.80 - 190 %7.80 - 190 %Average value: 77.6 % Grade Count:5
Elongation at Yield 2.60 - 2.90 %2.60 - 2.90 %Average value: 2.70 % Grade Count:3
Modulus of Elasticity 1.83 - 5.33 GPa265 - 773 ksiAverage value: 2.17 GPa Grade Count:25
Flexural Yield Strength 34.5 - 77.9 MPa5000 - 11300 psiAverage value: 59.2 MPa Grade Count:68
Flexural Modulus 1.23 - 2.55 GPa178 - 370 ksiAverage value: 1.99 GPa Grade Count:70
Compressive Yield Strength 5.90 - 52.0 MPa856 - 7540 psiAverage value: 46.3 MPa Grade Count:13
Bearing Yield Strength 20.3 - 359 MPa2940 - 52000 psiAverage value: 127 MPa Grade Count:12
Shear Strength 36.7 - 40.1 MPa5320 - 5820 psiAverage value: 38.3 MPa Grade Count:12
Izod Impact, Notched 1.46 - 5.34 J/cm2.74 - 10.0 ft-lb/inAverage value: 3.04 J/cm Grade Count:59
 0.461 - 2.99 J/cm
@Temperature -29.0 - -17.0 °C
0.864 - 5.60 ft-lb/in
@Temperature -20.2 - 1.40 °F
Average value: 1.37 J/cm Grade Count:44
Izod Impact, Unnotched 2.67 - 4.27 J/cm5.00 - 8.00 ft-lb/inAverage value: 3.63 J/cm Grade Count:10
 0.58729 - 2.1356 J/cm
@Temperature -40.0 - -40.0 °C
1.1002 - 4.0009 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.14 J/cm Grade Count:8
Gardner Impact 15.0 - 46.1 J11.1 - 34.0 ft-lbAverage value: 26.0 J Grade Count:14
 24.7 - 24.7 J
@Temperature -29.0 - -29.0 °C
18.2 - 18.2 ft-lb
@Temperature -20.2 - -20.2 °F
Average value: 24.7 J Grade Count:2
Falling Dart Impact 20.3 - 47.5 J15.0 - 35.0 ft-lbAverage value: 34.3 J Grade Count:9
 4.06746 - 31.1839 J
@Temperature -40.0 - -40.0 °C
3.00000 - 23.0000 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 14.6 J Grade Count:8
Instrumented Impact Total Energy 27.1 - 54.0 J20.0 - 39.8 ft-lbAverage value: 38.4 J Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.3 - 20.4 kV/mm414 - 518 kV/inAverage value: 17.8 kV/mm Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 44.5 - 101 µm/m-°C24.7 - 56.0 µin/in-°FAverage value: 85.7 µm/m-°C Grade Count:33
CTE, linear, Transverse to Flow 93.6 - 101 µm/m-°C52.0 - 56.0 µin/in-°FAverage value: 99.0 µm/m-°C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 82.2 - 105 °C180 - 221 °FAverage value: 92.7 °C Grade Count:50
Deflection Temperature at 1.8 MPa (264 psi) 77.8 - 106 °C172 - 222 °FAverage value: 89.3 °C Grade Count:43
Vicat Softening Point 107 °C225 °FAverage value: 107 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:55
 
Optical PropertiesMetricEnglishComments
Gloss 15.0 - 95.0 %15.0 - 95.0 %Average value: 65.4 % Grade Count:44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

O1150 / 77814

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.