MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials HiDura™ S3MG30H BK0835 Nylon PA610-GF30
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: HiDura S3MG30H BK0835 is a 30% glass fiber reinforced, heat stabilized polyamide 610 with 42% bio-based content for injection molding applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³DAM; ISO 1183
Water Absorption 0.400 %
@Time 86400 sec
0.400 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.00 %1.00 %from DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00300 cm/cm
@Thickness 2.00 mm
0.00300 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.00600 cm/cm
@Thickness 2.00 mm
0.00600 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi50%RH; ISO 527-2
 158 MPa22900 psiDAM; ISO 527-2
Elongation at Break 4.40 %4.40 %DAM; ISO 527-2
 7.60 %7.60 %50%RH; ISO 527-2
Tensile Modulus 6.80 GPa986 ksi50%RH; ISO 527-2
 9.10 GPa1320 ksiDAM; ISO 527-2
Flexural Strength 152 MPa22000 psi50%RH; ISO 178
 215 MPa31200 psiDAM; ISO 178
Flexural Modulus 6.20 GPa899 ksi50%RH; ISO 178
 8.40 GPa1220 ksiDAM; ISO 178
Poissons Ratio 0.3800.380ISO 527-2
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 180/1A
 12.0 kJ/m²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched  8.70 J/cm²
@Temperature -30.0 °C
41.4 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eU
 8.70 J/cm²
@Temperature -40.0 °C
41.4 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 179/1eU
 9.60 J/cm²
@Temperature -40.0 °C
45.7 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
 9.70 J/cm²
@Temperature -30.0 °C
46.2 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 9.70 J/cm²
@Temperature 23.0 °C
46.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 10.2 J/cm²
@Temperature 23.0 °C
48.5 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.20 J/cm²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
50%RH; ISO 179/1eA
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eA
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  29.0 kV/mm
@Thickness 1.00 mm
737 kV/in
@Thickness 0.0394 in
50%RH; IEC 60243
 32.0 kV/mm
@Thickness 1.00 mm
813 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.7 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 225 °C437 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 216 °C421 °F50%RH, Unannealed; ISO 75-2/B
 219 °C426 °FDAM, Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 193 °C379 °F50%RH, Unannealed; ISO 75-2/A
 197 °C387 °FDAM, Unannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 245 - 275 °C473 - 527 °FInjection
Middle Barrel Temperature 265 - 290 °C509 - 554 °FInjection
Front Barrel Temperature 270 - 300 °C518 - 572 °FInjection
Nozzle Temperature 275 - 305 °C527 - 581 °FInjection
Melt Temperature 255 - 300 °C491 - 572 °FInjection
Mold Temperature 70.0 - 100 °C158 - 212 °FInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
Agency RatingsASTM, D4066 PA0720A4306
 ASTM, D6779 PA0000A4356
 ISO, 1043 PA610 GF30
AppearanceBlack
FeaturesChemical Resistant
 Oil Resistant
 Solvent Resistant
FormsPellets
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8609 / 293358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.