MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 52G1 MX35 BLACK 51N PA 66/6, 35% Mineral Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Mineral Reinforced

Material Notes: Description: TECHNYL B 52G1 MX35 BLACK 51N is a 35% mineral fiber reinforced, halogen and red phosphorus free flame retarded grade based on copolyamide 66/6, for injection molding.

Key Properties: Glow wire resistance; Dimensional stability

Benefits: This grade offers glow wire resistance, dimensional stability, stability at high temperatures and good finishing.

Applications: It is used in all sector of industry, principally for pieces with low warping and good behavior at fire, as, for example, circuit breakers and boxes of fusers.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 75.0 MPa10900 psiISO 527 Type 1A
Elongation at Break 2.0 %2.0 %ISO 527 Type 1A
Tensile Modulus 10.4 GPa1510 ksiISO 527 Type 1A
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 6.00 GPa870 ksiISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.60 J/cm²7.61 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 245 °C473 °FISO 11357
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
ISO 1210
Glow Wire Test 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
Flammability Index; ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 270 °C500 - 518 °FCompression zone
 270 - 280 °C518 - 536 °FMixing zone
Feed Temperature 255 - 265 °C491 - 509 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVAY855 / 218583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.