MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kohesi Bond KB 1686 M Two component, nickel filled, electrically conductive epoxy for bonding and sealing
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes: Product Highlights:
  • Easy mix ratio of 1:1 by weight or volume
  • Outstanding dimensional stability
  • Superior thermal conductivity
  • High lap shear strength (> 2,100 psi)
  • Nickel filled, electrically conductive
  • 100% solids system
Kohesi Bond KB 1686 M is a two component, nickel filled epoxy system suitable for bonding, coating and sealing. It has a convenient 1:1 (Part A: Part B) mix ratio by weight or volume. Firstly, it offers very good electrical conductivity and dimensional stability. This epoxy system readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1686 M offers a volume resistivity of 5 - 10 ohm-cm. It is ideal for use in static dissipation and EMI/RFI shielding applications. It offers an extensive service temperature range of -50°C to +120°C. It is an outstanding adhesive that offers superb physical strength properties, allowing it to adhere well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical and thermal conductivity (1.3 - 1.4 W/m/K), it also offers excellent chemical resistance to various cleaning agents, oils and water. Part A and Part B are gray in color. It has a thixotropic paste like consistency and a very low coefficient of thermal expansion (CTE). Owing to its versatile performance, KB 1686 M is widely used in electronics, aerospace, electrical, semiconductor, microwave and many OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Coating

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity >= 510000 cP>= 510000 cPPart A, thixotropic
 >= 905000 cP>= 905000 cPPart B, thixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 42.1 MPa>= 6100 psi
Tensile Modulus >= 3.52 GPa>= 510 ksi
Compressive Strength >= 159 MPa>= 23000 psi
Adhesive Bond Strength >= 14.5 MPa>= 2100 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.0 - 10 ohm-cm5.0 - 10 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 - 35.0 µm/m-°C13.9 - 19.4 µin/in-°F
Thermal Conductivity 1.50 - 1.60 W/m-K10.4 - 11.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Option 2
 180 - 300 min
@Temperature 70.0 - 90.0 °C
3.00 - 5.00 hour
@Temperature 158 - 194 °F
Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
 4320 - 7200 min
@Temperature 23.0 °C
72.0 - 120 hour
@Temperature 73.4 °F
Option 1
Working Life >= 120 min>= 120 min100 g of mixed epoxy
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Monthin original unopened containers
 
Descriptive Properties
Mixing Ratio1:1 by weight or volumePart A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI963 / 249142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.