MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rotuba MSS Cellulose Acetate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: Property values at 50% RH.

Data provided by the manufacturer.

Key Words: Rotuba Plastics; Cellulosic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D792
Water Absorption 2.5 %2.5 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 3131ASTM D785
Tensile Strength, Ultimate 27.0 MPa3920 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 53 %53 %ASTM D638
Flexural Yield Strength 27.0 MPa3920 psiASTM D790
Flexural Modulus 0.0800 GPa11.6 ksiASTM D790
Izod Impact, Notched 3.52 J/cm6.59 ft-lb/inASTM D256
 0.690 J/cm
@Temperature -40.0 °C
1.29 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 138 °C280 °FFlow temperature, ASTM D569
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 °C356 °FCenter barrel temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 121241 B Bio-Based Polylactic Acid (PLA); PC-PLA Blend - ESD Protection - Permanently Anti-static - 26% Renewable Resource Content
RTP Company RTP 199 X 143685 A Polypropylene (PP); Copolymer - Cellulose Fiber - 20% Renewable Resource Content
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp
Celanese Riteflex® 655A TPC, Unfilled

PECR08 / 35484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.