MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Miracll C85 Polycarbonate-based TPU, C Series
Categories: Polymer; Thermoplastic; Polyurethane, TP; Polycarbonate-Urethane

Material Notes: Excellent aging resistance, oil resistance, hydrolysis resistance, high temperature resistance, UV resistance, excellent physical properties & weathering resistance, etc. Applications: hose & tube, film & sheet, fire hose, oil tank.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
ASTM D412
300% Modulus 16.0 MPa
@Strain 300 %
2320 psi
@Strain 300 %
ASTM D412
Tear Strength 100 kN/m571 pliASTM D624
Abrasion 2525DIN Abrasion Loss; DIN 53516
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -25.0 °C-13.0 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Pellethane® 2363-90AE TPU
Lubrizol LifeSciences Carbothane® AC-4085A-B20 Aromatic TPU
Lubrizol LifeSciences Carbothane® AC-4085A TPU – Clear Aromatic
Lubrizol Estane® S190A Thermoplastic Polyurethane
Lubrizol Estane® S185A Thermoplastic Polyurethane

PMIRAC81 / 221410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.