MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik EUROPLEX® PPSU 99470 KR/DF Transparent sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: EUROPLEX® PPSU is a flame-retardant sheet material based on polyphenylsulfone (PPSU). It shows excellent mechanical properties as well as good chemical resistance. The sheet series meets the fire standard requirements for many applications in public transport including the OSU 65/65 heat release requirements for large interior parts in passenger aircraft. EUROPLEX ® PPSU sheets are available in transparent and opaquely colors.

EUROPLEX® PPSU 99470 KR/DF transparent with functional coating: The EUROPLEX® PPSU transparent sheet grades can be provided with a functional coating. Different systems can be applied, such as high scratch resistance (KR) or white light-scattering coating (DF). Functional coating for EUROPLEX® PPSU transparent sheet provide hardness, nonglare light-scattering surfaces combined with improved climatic resistance.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Elongation at Break 60 - 80 %60 - 80 %ISO 527
Modulus of Elasticity 2.30 GPa334 ksiISO 527
Charpy Impact Unnotched NBNBISO 179
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 195 °C383 °F
Vicat Softening Point 223 °C433 °FISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Evonik EUROPLEX® PPSU Sheet
Evonik Europlex® PPSU Polyphenylsulfone Engineering Plastic
Evonik EUROPLEX® PPSU 99470/99472 Transparent sheet
Ensinger TECASON™ P Polyphenylsulfone (PPSU)

PEVONIL150 / 196354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.