MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AGY ZenTron® S-2 Generic S-Glass Fiber
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Moderate alkali resistance.

Information provided by AGY Holding Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.48 g/cc0.0896 lb/in³
Density 2.46 g/cc0.0889 lb/in³
Water Absorption 0.00 %0.00 %
Loss On Ignition 0.10 - 1.4 %0.10 - 1.4 %Varies according to size type
Filament Diameter 5.0 - 25 µm5.0 - 25 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  4445 MPa
@Temperature 371 °C
644700 psi
@Temperature 700 °F
 4890 MPa
@Temperature 23.0 °C
709000 psi
@Temperature 73.4 °F
Elongation at Break 5.7 %5.7 %in 50 mm
Modulus of Elasticity 86.9 GPa12600 ksi
Poissons Ratio 0.220.22
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 9.05e+12 ohm-cm9.05e+12 ohm-cm
Dielectric Constant  5.2
@Frequency 1e+10 Hz
5.2
@Frequency 1e+10 Hz
 5.3
@Frequency 1e+6 Hz
5.3
@Frequency 1e+6 Hz
Dielectric Strength 18.0 kV/mm457 kV/in
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.60 µm/m-°C
@Temperature -30.0 - 250 °C
0.889 µin/in-°F
@Temperature -22.0 - 482 °F
average, isotropic
Specific Heat Capacity  0.737 J/g-°C
@Temperature 23.0 °C
0.176 BTU/lb-°F
@Temperature 73.4 °F
 0.935 J/g-°C
@Temperature 200 °C
0.223 BTU/lb-°F
@Temperature 392 °F
Thermal Conductivity 1.10 - 1.40 W/m-K7.63 - 9.72 BTU-in/hr-ft²-°F
Melting Point 1466 °C2671 °FLiquidus
Liquidus 1466 °C2671 °F
Maximum Service Temperature, Air 875 °C1610 °FWell above Tg, due to reversible phase separation
Maximum Service Temperature, Inert 875 °C1610 °F
Transformation Temperature, Tg 845 °C1550 °F
Softening Point 1056 °C1933 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5211.521
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
S-2 Glass® Fiber
S-Glass Fiber, Generic
A-Glass Fiber, Generic
E-Glass Fiber, Generic
AGY ADVANTEX® Generic Glass Fiber

CGLASS00 / 930

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.