MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials HCM Boron Nitride (BN) Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap densities of ~1 g/cm3. These features, combined with low average surface areas, give powders that flow readily, withstand harsh processing, and have outstanding thermal characteristics.

HCM has a slightly finer average particle size of 175 µm and is processed for outstanding purity, making it appropriate for the most demanding of applications. HCM also has a more uniform particle size distribution and rounded particles due to its unique processing.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.00 g/cc0.0361 lb/in³Tap Density
Particle Size 10 µm10 µmCrystal Size
 175 µm175 µmMean
Specific Surface Area 2.0 m²/g2.0 m²/g
 
Descriptive Properties
Carbon0.03%
ColorWhite
Crystal TypeHexagonal (Graphitic)
Oxygen0.3%
Sol. Borate0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tellurium, Te
Titanium Nitride (TiN) Coating
MarkeTech Gallium Arsenide Semiconductor Wafer, p-type, Zinc Doped, LEC Grown
MarkeTech Gallium Arsenide Semiconductor Wafer, n-type, Tellurium Doped, LEC Grown
MarkeTech Gallium Arsenide Semiconductor Wafer, n-type, Silicon Doped, HB-GF Grown

CADV19 / 411

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.