MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surface and differentiates HALAR® from other fluoropolymers. Due to the fact that ECTFE is very pure, this material is being used to process chemicals and ultrapure water for the semiconductor industry. Also, the permeation resistance to oxygen, carbon dioxide, chlorine gas and hydrochloric acid is 10 to 100 times better than PTFE.

Properties

  • extremely high impact strength
  • good insulation properties
  • very good weather resistance
  • high resistance to radiation
  • very high chemical resistance
  • very good sliding properties
  • physiologically harmless
  • high density
  • non-consistent against hot amines
Applications includes parts which come in contact with aggressive materials, lining of tanks, pumps, flanges, fittings, parts in centrifuges and control engineering industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.71 g/cc1.71 g/ccISO 1183
Water Absorption at Saturation 0.70 %0.70 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ISO 868
Ball Indentation Hardness 90.0 MPa13100 psiR; ISO 2039
Tensile Strength at Break 47.0 MPa6820 psiISO 527
Tensile Strength, Yield 30.0 MPa4350 psiISO 527
Elongation at Break 250 %250 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Modulus of Elasticity 1.845 GPa267.6 ksiISO 527
Flexural Strength 54.0 MPa7830 psiISO 178
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmIEC 60093
Dielectric Constant 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm381 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FISO 11359
Thermal Conductivity 0.150 W/m-K
@Temperature 20.0 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ISO 22007-4
Melting Point 230 °C446 °FDIN EN ISO 3146
Maximum Service Temperature, Air 150 °C302 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FISO 75
Minimum Service Temperature, Air -76.0 °C-105 °FUL 746B
Glass Transition Temp, Tg 85.0 °C185 °FDIN EN ISO 3146
Flammability, UL94 V-0V-0UL 94
Oxygen Index 52 %52 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA NoNoPhysiological indifference
 
Descriptive Properties
Acid Resistancelimited
Aromatic Resistanceyes
Bondabilitylimited, pretreatment necessary
CKW Resistanceyes
Colornatural
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Physiological indifferenceno, EEC
Resistance Against Hot Wateryes
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe PA 66 Nylon 66
3M Dyneon™ ET 6235Z Fluorothermoplastic Granules
Isoflon ETFE
Isoflon ECTFE Fluoropolymer
Hippe PEI

PGEHR031 / 79868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.