MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® STAT A 20 FC BK PA66-CF20
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: Vydyne STAT A 20 FC BK is standard flow, 20% carbon-fiber reinforced PA66 resin. This product shows high stiffness and strength. It is also electrically conductive.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
0.0020 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
@Thickness 2.00 mm
0.0040 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiDAM; ISO 527-2
Elongation at Break 2.0 %2.0 %DAM; ISO 527-2
Tensile Modulus 13.0 GPa1890 ksiDAM; ISO 527-2
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm
@Thickness 1.00 mm
1000 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 295 °C518 - 563 °FInjection
Middle Barrel Temperature 275 - 295 °C527 - 563 °FInjection
Front Barrel Temperature 280 - 300 °C536 - 572 °FInjection
Nozzle Temperature 280 - 300 °C536 - 572 °FInjection
Melt Temperature 280 - 295 °C536 - 563 °FInjection
Mold Temperature 70.0 - 90.0 °C158 - 194 °FInjection
Drying Temperature 80.0 - 110 °C176 - 230 °FInjection
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
Agency RatingsISO, 1043 PA66 20CF
AppearanceBlack
FeaturesBromine Free
 Chemical Resistant
 General Purpose
 Good Dimensional Stability
 Good Electrical Properties
 Good Processability
 Good Rigidity
 Good Stiffness
 Good Strength
 Good Tensile Strength
 Halogen Content, None
 Homopolymer
 Lubricated
 Medium Viscosity
 Non-Corrosive
 Oil Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8548 / 296308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.