MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 10% Glass Fiber Reinforced; Nylon 66/6, Mineral Reinforced

Material Notes: Mixed products with improved stiffness and good dimensional stability, low warpage.

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080Conditioned; ISO 868
 8484ISO 868
Tensile Strength at Break 60.0 MPa8700 psiConditioned; ISO R 527
 105 MPa15200 psiISO R 527
Elongation at Yield 5.0 %5.0 %ISO R 527
 9.0 %9.0 %Conditioned; ISO R 527
Modulus of Elasticity 3.50 GPa508 ksiConditioned; ISO 178
 7.50 GPa1090 ksiISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²2.62 ft-lb/in²ISO 180/1A
 7.00 kJ/m²3.33 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/IeU
 6.00 J/cm²28.6 ft-lb/in²Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/IeA
 0.700 J/cm²3.33 ft-lb/in²Conditioned; ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; CEI 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmCEI 60093
Comparative Tracking Index 600 V600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FASTM E831
Melting Point 243 °C469 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-2/AF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6
Ravago Manufacturing Americas Hylon N5116MGHL Nylon 66, 8% Mineral, 8% Glass Filled, DAM
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
Copper, Cu; Cold-Worked

PFADD893 / 156107

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.