MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E40654. 00714 is available in brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.720 g/cc0.0260 lb/in³ASTM D1895
Density 1.65 g/cc0.0596 lb/in³ASTM D792
Water Absorption 0.286 %0.286 %ASTM D570
Linear Mold Shrinkage 0.0068 cm/cm0.0068 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7171ASTM D785
Tensile Strength, Ultimate 62.0 MPa8990 psiASTM D638
Elongation at Break 0.70 %0.70 %ASTM D638
Tensile Modulus 11.0 GPa1600 ksiASTM D638
Flexural Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 9.90 GPa1440 ksiASTM D790
Compressive Strength 151 MPa21900 psiASTM D695
Poissons Ratio 0.310.31ASTM D638
Shear Modulus 4.20 GPa609 ksiCalculated
Izod Impact, Notched 0.159 J/cm0.298 ft-lb/inASTM D256
Charpy Impact, Notched 0.165 J/cm²0.785 ft-lb/in²ASTM D256
Impact 8585J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.70e+12 ohm-cm3.70e+12 ohm-cmASTM D247
Dielectric Constant 6.96.9ASTM D150
Dielectric Strength 6.30 kV/mm160 kV/inStep by Step; ASTM D149
 9.50 kV/mm241 kV/inShort Time; ASTM D149
Dissipation Factor 0.0690.069ASTM D150
Arc Resistance 186 sec186 secASTM D495
Comparative Tracking Index 575 V575 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C
@Temperature 40.0 - 130 °C
28.9 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 142 °C288 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.90 %0.90 %240 hr, 105ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded
Overview of materials for Melamine-Phenolic Copolymer
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded

PLEL00 / 50568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.